C17200 (UNS C17200, CuBe2, 2.1247) is the strongest copper alloy in routine industrial use — about 1,200 MPa tensile at 38 HRC after ageing — and it does something no stainless can: it conducts heat and electricity while staying non-magnetic. In MWD and logging tools that combination is what keeps electronics cool inside a non-magnetic housing.

C17200 beryllium copper bar and tube for non-magnetic downhole components
Aged hardness 36–42 HRC; alloy Copper-beryllium, age hardened.
UNS designationC17200
Alloy familyCopper-beryllium, age hardened
Primary standardASTM B196 / B643
Hardness (aged)36–42 HRC

The alloy carries 1.80–2.00% beryllium, which is soluble in copper at high temperature and precipitates as fine particles on ageing at 300–340 °C. That is what takes a soft, workable metal to a hardness comparable with 17-4PH while retaining copper’s conductivity, roughly 22% IACS in the aged condition against 2% for stainless.

For downhole tools the practical advantages are thermal management, non-magnetic behaviour and galling resistance. Bearings, bushings and wear surfaces in MWD tools are frequently C17200 running against stainless or against itself, because the pair does not seize the way two stainless parts do.

The handling caution is real: beryllium-bearing dust from grinding and machining is a health hazard, and shops must control it. Finished solid components present no such risk, but the purchase specification should say whether machining swarf will be returned.

Standards and Tempers

ASTM B196 covers rod and bar, B643 covers tube, and B194 covers plate and strip. Tempers run from solution annealed (A) through quarter-hard to hard, with the aged condition (AT) supplied either by the mill or produced after machining. Mechanical properties depend on temper, so the order must state it.

System Designation
UNS C17200
W.Nr. / EN 2.1247 / CuBe2
ASTM B196 Rod and bar
ASTM B643 Tube
ASTM B194 Plate, sheet, strip
Tempers A, 1/4H, 1/2H, H, AT (aged)

Where C17200 Is Used

MWD and LWD housings

Non-magnetic electronics carriers where heat must be conducted away from instruments.

Bearings and bushings

Non-magnetic sleeve bearings and wear rings running against stainless shafts without galling.

Springs and contacts

Electrical contacts, leaf springs and connectors that must survive vibration at temperature.

Valve seats and seals

Seat inserts and seal rings where a soft metal has to conform to a harder face.

Spark-free tooling

Hand tools and fixtures used in explosive atmospheres, where steel sparks are unacceptable.

Heat sinks and cold plates

Thermal management components inside instrument packages.

Supply Range and Condition

Round bar from 6 mm to 150 mm diameter, tube from 6 mm to 80 mm outside diameter, and plate to 100 mm. Supplied solution annealed for machining, or aged to the specified temper where the part is finish-machined before delivery.

Testing includes chemistry with beryllium and cobalt reported per heat, hardness and tensile by temper, and conductivity where specified. EN 10204 3.1 certificates with heat traceability.

Chemical Composition of C17200 (wt%)

Beryllium at 1.80–2.00% is the alloy’s defining element and must be reported on the certificate. Cobalt or nickel at 0.20% minimum is a deliberate addition that refines the precipitate and slows over-ageing; the combined Co + Ni + Fe is capped at 0.60%.

Element Min % Max %
Beryllium (Be) 1.80 2.00
Cobalt + Nickel (Co+Ni) 0.20 —
Cobalt + Nickel + Iron — 0.60
Copper (Cu) balance balance
Aluminium (Al) — 0.20
Silicon (Si) — 0.20
Lead (Pb) — 0.02

Mechanical Properties by Temper

Values are typical for the two conditions most often ordered. Ageing is carried out at 300–340 °C for 2–3 hours after machining; the part shrinks slightly during ageing, so allowances must be built into the drawing.

Condition Tensile strength Yield (0.2%) Elongation Hardness
Solution annealed 480–560 MPa 200–380 MPa 35–60% ≤ 20 HRC
Aged (AT) 1,100–1,400 MPa 965–1,240 MPa 3–10% 36–42 HRC

Need C17200 bar or tube in a specific temper?

Send the size, temper, quantity and whether ageing is done before or after machining — we reply with mill availability, lead time and a priced offer, usually within one working day.

Request a quotationWhatsApp +86 178 7358 1838