Alloy 20 (UNS N08020, 20Cb-3, W.Nr. 2.4660) is an austenitic nickel-iron-chromium alloy with 3–4% copper and a niobium addition. It exists for one family of duties: sulphuric acid, and mixtures of sulphuric acid with nitric or hydrochloric acid, where 316L and 904L corrode too fast and a full nickel alloy is more than the process requires.

The copper addition is what makes the grade work in sulphuric acid: it shifts the corrosion potential so the alloy passivates in the 20–90% concentration range at moderate temperature, and it keeps that passivity in diluted acid where the concentration swings during washing or shutdown. Across the same range 316L shows active corrosion at rates that make a 3 mm allowance pointless.
The niobium addition (8 × carbon minimum, up to 1.0%) stabilises the alloy against intergranular attack in the weld heat-affected zone. Without it, welded acid lines suffer knife-line attack along the fusion boundary — a failure mode that looks like a manufacturing defect but is really a chemistry selection error.
In refining, Alloy 20 is the standard material for sulphuric acid alkylation unit internals, acid coolers, and spent acid recovery. Outside refining it appears in pickling lines, acid storage and transport, and fertiliser plants. It is not a seawater alloy and it is not a caustic chloride alloy — for those, 904L, 6Mo or a nickel alloy is the right answer.
Alloy 20 Standards and Equivalent Grades
Each product form has its own ASTM specification: B473 for bar and wire, B729 for seamless pipe and tube, B464 for welded pipe, B463 for plate and sheet, and B366 for fittings. The grade is also covered by DIN 17744 and by NACE MR0175 for sour service, though it is rarely selected for that duty.
| System | Designation |
| UNS | N08020 |
| W.Nr. / DIN | 2.4660 / NiCr20CuMo |
| Common trade names | 20Cb-3, Carpenter 20, CN7M (cast) |
| ASTM B473 | Bar and wire |
| ASTM B729 | Seamless pipe and tube |
| ASTM B464 / B463 | Welded pipe / plate and sheet |
| ASTM A351 CN7M | Cast equivalent for valve bodies |
Where Alloy 20 Is Specified
Sulphuric acid alkylation
Reactor internals, acid coolers, settler components and acid circulation lines in HF and sulphuric alkylation units.
Spent acid recovery
Concentrators, reboilers and transfer lines handling hot 70–93% acid with dissolved organics.
Pickling and plating lines
Hooks, baskets, heat exchanger coils and tank linings in sulphuric-nitric pickling baths.
Acid storage and transport
Tank shells, dip pipes, tanker fittings and pumps for 98% acid and for dilute acid that cycles in concentration.
Heat exchanger tubing
Tube bundles for acid coolers and interchangers, where 904L shows unacceptable wall loss at the hot end.
Pump and valve internals
Shafts, sleeves, impellers and trim in acid transfer service; cast CN7M bodies are matched to wrought internals.
Supply Range and Delivery Condition
Round bar from 16 mm to 300 mm diameter, peeled or ground; seamless pipe from 6 mm to 219 mm outside diameter; seamless tube from 6 mm to 50 mm; forged blocks and flanges to drawing. Standard condition is solution annealed at 940–1,010 °C and water quenched, pickled and passivated.
Testing includes chemistry with copper and niobium reported per heat, tensile and hardness, intergranular corrosion test to ASTM A262 Practice B or E where specified, and hydrostatic or eddy current testing on pipe. EN 10204 3.1 certificates with heat traceability as standard.
Chemical Composition of Alloy 20 (wt%)
Copper at 3.0–4.0% and niobium at 8 × carbon minimum are the two elements that define the grade; a heat without either is not Alloy 20 regardless of what the certificate is titled. Carbon is capped at 0.07% to limit the niobium required for stabilisation.
| Element | Min % | Max % |
| Nickel (Ni) | 32.00 | 38.00 |
| Chromium (Cr) | 19.00 | 21.00 |
| Copper (Cu) | 3.00 | 4.00 |
| Molybdenum (Mo) | 2.00 | 3.00 |
| Niobium + Tantalum (Nb+Ta) | 8 × C | 1.00 |
| Carbon (C) | — | 0.070 |
| Manganese (Mn) | — | 2.00 |
| Silicon (Si) | — | 1.00 |
| Phosphorus (P) | — | 0.045 |
| Sulphur (S) | — | 0.035 |
| Iron (Fe) | balance | balance |
Mechanical Properties of Alloy 20
Values are the ASTM B473 minima for solution-annealed bar at room temperature; pipe to B729 is comparable. The grade is not hardenable by heat treatment and is used annealed throughout.
| Property (room temperature) | ASTM B473 minimum |
| Tensile strength | ≥ 550 MPa |
| Yield strength (0.2%) | ≥ 240 MPa |
| Elongation in 50 mm | ≥ 30% |
| Hardness | ≤ 95 HRB |